Reagents, G, UN2265
1 - 2 of 2
Sort
View
Show
-
•Graphene preparation method: electrochemical exfoliation. •Graphene thickness by AFM: 80%, 1-3 layers. •Sheet size by AFM: 10 mum. •Oxygen content: 7.5% (by XPS) (C/O-ratio: 12.3). •Raman I_D/I_G ratio: 0.4. •Sheet resistance: 4.8 kOmega/sq. •Typical properties of films produced thereof…
-
Graphene/PEDOT:PSS hybrid ink dispersion in DMF
MilliporeSigma•Graphene preparation method: Electrochemical exfoliation. •Graphene thickness by AFM: 80%, 1-3 layers. •Sheet size by AFM: 10 mum. •Oxygen content: 7.5% (by XPS) (C/O-ratio: 12.3). •Raman I_D/I_G ratio: 0.4. •Sheet resistance: 4.8 kOmega/sq. •Typical properties of films produced thereof…